Products
- Nickel[10]
- Stainless Steel Bars[10]
- Stainless Steel Flats[3]
- Stainless Steel Pipes[2]
- Stainless Steel Sheets[3]
- Stainless Steel Strips[2]
- Stainless Steel Wire[1]
- Flat Steel[1]
- Steel Round Bars[10]
- Steel Sheets[4]
- Structural Steel[8]
- Titanium Wire[1]
Contact Us
- Contact Person : Mr. Guo Daojin
- Company Name : Sichuan Jiangyou Singular New Material Development Co., Ltd.
- Tel : 86-0816-3220015
- Fax : 86-0816-3220015
- Address : Sichuan,Jiangyou Sichuan,(No.2-2 first floor,71 buliding living area,the third factory of ChangGang)Hanzeng Town of Jiangyou
- Country/Region : China
- Zip : 621700
Product Detailed
Related Categories:Stainless Steel Bars
Related Product Searches:Hastelloy C-4 /N06455 superalloy tube/pipe,High Quality,Hastelloy C-4, hastelloy c276 tube,tube/pipe
1.round bar diameter:8-2000mm.
2.plate/sheet thickness:2-200mm.
3.forgings weight:0.5-10000Kg.
4.pipe/tube OD6-3500mm.
Related Product Searches:Hastelloy C-4 /N06455 superalloy tube/pipe,High Quality,Hastelloy C-4, hastelloy c276 tube,tube/pipe
1.Type analysis
C | Si | Mn | Cr | Mo | Ti | Fe | S | Co | Ni |
0.015 | 0.08 | 1.0 | 14-18 | 14-17 | 0.7 | 3 | 0.030 | 2.0 | balance |
2.Description
HASTELLOY C-4 alloy is a nickelchromium- molybdenum alloy with outstanding high-temperature stability, as evidenced by high ductility and corrosion resistance even after longtime aging at 1200 to 1900 deg. F (649 to 1038 deg. C). The alloy also has excellent resistance to stress corrosion cracking and to oxidizing atmospheres up to 1900 deg. F (1038 deg. C).
Hastelloy C-4 /N06455 superalloy tube/pipe